Desliming Test on a Weathering Domestic Titanium Ore Dressing Plant

SHEN Xu,ZHANG Hanping   

  1. Faculty of Mining Engineering, Kunming Metallurgy College, Kunming 650033,China
  • Received:2016-04-13 Online:2016-07-23 Published:2016-07-23

Abstract:

     Pilot-plant-scale tests of “desliming-spiral chute re-election” with inclined plane thickener have been conducted in a typical domestic laterite weathering titanium plant. Good test indicators are achieved: 1) amount of clay removal can reach 55%~60%, TiO2 in clay is only 0.5%~0. 9% and the loss rate of metal in mud is only 5% to 8% by using high efficiency inclined plate thickener; 2) after desliming, the same spiral chute was used to gravity separation. The content of TiO2 in concentrate can reach 33.54%, and the recovery rate is 86.58%; 3) the process is simple, the production operation is feasible by using the high efficiency inclined plate thickener; 4) the results of this study can provide reliable technical support for the technological transformation of the mineral processing plant.

Key words: weathering titanium ore, high efficient inclined plate thickener, desliming